1 (a)
Define atomic packing factor and calculate atomic radius and packing factor for BCC structure
8 M
1 (b)
With a neat sketch,expalin the line dislocation
6 M
1 (c)
State and explain the fick's second law of diffusion.
6 M
2 (a)
With the help of a neat schematic conventional stress diagram for mild steel under tension,explain clearly the behaviour of the material till fracture
6 M
2 (b)
Expalin non-linear elastic properties when a material is subjected to static tension
6 M
2 (c)
What is work hardening?Explain the reasons for the same
6 M
3 (a)
Explain with neat figure ductile feature using both stress strain and stages of fracture
8 M
3 (b)
What is mean by stress relaxation ?Explain with figure
6 M
3 (c)
With the help of sketch,discuss the different types of stress cycles which bring about fatigue failure
6 M
4 (a)
Explain with neat sketches the different stages of mechanism of solidification
8 M
4 (b)
Define solid solution .Explain the substitutional and interstiatial solid solution
8 M
4 (c)
Explain the factor governing the formation of substitutional solid solution
4 M
5 (a)
Draw and explain the Iron -Iron carbide equilibrium diagram and label all the points and field
10 M
5 (b)
Consruct a phase digram using the following data and label all the fields ;
Melting point of ag =961°C
Melting point of Cu =1083°C ,
Eutectic tempreture =780°C
Eutectic compostion =28%Cu
Max solubility of Cu in Ag=9% at 780°C
max.solubilty of c in Ag =2%at 0°C
Max.solubilty of Cu in Ag =9% at 780°c
Max.solubilty of cu in Ag =0% at 0°C.
Detemine the following ;
solidfication start and end solid tempreture for 30% Ag alloy.
TEmpreture at which a 15% Cu alloy has 50% liquid phase and 50% solid phase
Percentage composition of liquid and solid phase 20% Ag alloy at 900°C
Melting point of ag =961°C
Melting point of Cu =1083°C ,
Eutectic tempreture =780°C
Eutectic compostion =28%Cu
Max solubility of Cu in Ag=9% at 780°C
max.solubilty of c in Ag =2%at 0°C
Max.solubilty of Cu in Ag =9% at 780°c
Max.solubilty of cu in Ag =0% at 0°C.
Detemine the following ;
solidfication start and end solid tempreture for 30% Ag alloy.
TEmpreture at which a 15% Cu alloy has 50% liquid phase and 50% solid phase
Percentage composition of liquid and solid phase 20% Ag alloy at 900°C
10 M
6 (a)
Draw the TTT digram of austentie for eutectoid steel.Explain the various trasnsmission product of austenite
8 M
6 (b)
Discuss the process tempreture range range,microstructure of products and application of stress relif annealing
6 M
6 (c)
Expalin with neat sketch induction hardening process
6 M
7 (a)
Give the compostion,structure and their application of
S.G iron
Malleable Iron
Gray cast Iron
S.G iron
Malleable Iron
Gray cast Iron
8 M
7 (b)
Name at least four important copper base alloys.Give Compostition microstructure and their application
8 M
7 (c)
Write a note on AL-Si alloys
4 M
8 (a)
Explain the term composite material with example.State their advantages limitation of composites in practice
8 M
8 (b)
Usin neat sketch ,explain the process of preparation of metal matrix composite using melting and casting method
8 M
8 (c)
What are FRPs?Give at least four example
4 M
More question papers from Material Science & Metallurgy